Nickel 200/201 strips and shims find widespread use in applications where corrosion resistance, temperature stability, and electrical conductivity are paramount, including the fabrication and maintenance of equipment in various industrial settings. The choice between Nickel 200 and Nickel 201 depends on specific purity requirements, with Nickel 201 offering the highest level of nickel purity.
Nickel 200/201, which are commercially pure nickel grades, find applications in various industries due to their excellent corrosion resistance and high thermal and electrical conductivity. In the context of lithium batteries, these nickel grades can be utilized in the form of strips and shims for specific purposes:
At Satyam Overseas, we prioritize Material Certification and Traceability. Our materials, meeting ASTM and ASME standards, come with 3.1 Mill Test Certificates as a guarantee of compliance. Additionally, upon request, we provide 3.2 Mill Test Certificates for added assurance. Every material is clearly marked and accompanied by a corresponding certificate, meticulously linking markings to certification. This meticulous approach ensures complete accountability and unwavering reliability throughout our supply chain.
Nickel | Copper | Iron | Manganese | Carbon | Silicon | Sulfur | |
---|---|---|---|---|---|---|---|
Min | 99.0 | – | – | – | – | – | – |
Max | – | 0.25 | 0.40 | 0.35 | 0.15 | 0.35 | 0.01 |
Nickel | Copper | Iron | Manganese | Carbon | Silicon | Sulfur | |
---|---|---|---|---|---|---|---|
Min | 99.0 | – | – | – | – | – | – |
Max | – | 0.25 | 0.40 | 0.35 | 0.02 | 0.35 | 0.01 |
Density, lb/in 3 | Density, g/cm 3 | Melting Range, °F | Melting Range, °C | Specific Heat, Btu/lb•°F | Specific Heat, J/kg•°C | Curie Temperature, °F | Curie Temperature, °C |
---|---|---|---|---|---|---|---|
0.321 | 8.89 | 2615-2635 | 1435-1446 | 0.109 | 456 | 680 | 360 |
Density, lb/in 3 | Density, g/cm 3 | Specific Heat, Btu/lb•°F | Specific Heat,J/kg•°C | Curie Temperature, °F | Curie Temperature, °C | Modulus of Elasticity (Tension), 103 ksi | Modulus of Elasticity (Tension), GPa |
---|---|---|---|---|---|---|---|
0.321 | 8.89 | 0.109 | 456 | 680 | 360 | 60 | 207 |