Inconel 601 Sheets & Plates are crucial materials known for their outstanding properties, making them invaluable in various high-temperature and corrosive environments. Composed of nickel, chromium, and other elements, Inconel 601 exhibits remarkable resistance to oxidation and corrosion at elevated temperatures, making it ideal for applications in heat treatment, chemical processing, and furnace components.
These plates and sheets can withstand temperatures of up to 2200°F (1204°C) while maintaining their integrity, offering exceptional thermal stability in demanding conditions. Furthermore, their mechanical properties, including high tensile strength and excellent ductility, ensure they can endure mechanical stresses and remain reliable in critical applications.
In addition to their heat resistance, Inconel 601 plates and sheets exhibit good thermal conductivity, which is advantageous in heat exchangers and other heat transfer applications. Their adherence to industry standards, often specified under ASTM B168, guarantees consistent quality and performance. This combination of features positions Inconel 601 as a trusted choice in industries where high-temperature capabilities and corrosion resistance are paramount.
At Satyam Overseas, we prioritize Material Certification and Traceability. Our materials, meeting ASTM and ASME standards, come with 3.1 Mill Test Certificates as a guarantee of compliance. Additionally, upon request, we provide 3.2 Mill Test Certificates for added assurance. Every material is clearly marked and accompanied by a corresponding certificate, meticulously linking markings to certification. This meticulous approach ensures complete accountability and unwavering reliability throughout our supply chain.
Ni | Cr | Fe | AI | C | Mn | S | Si | Cu | |
---|---|---|---|---|---|---|---|---|---|
Min | 58 | 21 | - | 1 | 0.03 | - | - | - | - |
Max | 63 | 25 | 18 | 1.7 | 0.1 | 1 | 0.015 | 0.5 | 0.5 |
Density | Melting range | Relative magnetic permeability at 20 °C (68 °F) | Curie temperature |
---|---|---|---|
8.05 g/cm3 (0.29 lb/in3 ) | 1,330-1,370 °C (2,426-2,498 °F) | 1.01 (Maximum) | -196 °C (Maximum) (-320.8 °F) |
Forms | ASTM | ASME | DIN |
---|---|---|---|
Sheet, plate | B 168 | SB 168 | 17742 17750 |
Inconel and Hastelloy are both nickel-chromium-molybdenum-based alloys. They are all corrosion-resistant and extremely strong metals. Hastelloy has greater molybdenum content than Inconel, although Inconel has a higher chromium concentration. This sets them apart in terms of corrosion resistance in different situations.